Surprisingly, I have some stuff that has been fired, that still has pencil on the bottom.  We wrote numbers and took photos before firing.  Most surprised to see pencil marks still there.

So, is it matters, remove before firing.

Share this post


Link to post
Share on other sites

Sometimes you don't want the lines or marks to go away...I mark all my pieces with a code (or serial #) that corresponds to a drawing and photo with a description of the glaze process used to achieve a particular look. This allows me to go back into my files to regenerate a look that a customer likes on a new piece. The code is written with a glaze pencil and doesn't burn off...

696554128_Codesample1.jpg.890a4bba9bf1746ed817e7d0b4326fad.jpg526027800_Codesample2.jpg.eaf17e3fa22f487481f903279c5901e8.jpg864681798_Codesample3.jpg.38b9c36141c705dd3bf91256a41bfe28.jpg

Share this post


Link to post
Share on other sites
On 11/7/2019 at 8:37 PM, Chilly said:

Surprisingly, I have some stuff that has been fired, that still has pencil on the bottom.  We wrote numbers and took photos before firing.  Most surprised to see pencil marks still there.

So, is it matters, remove before firing.

Was it a coloured pencil?

Black instead of a "lead"?

Share this post


Link to post
Share on other sites
1 hour ago, Babs said:

Was it a coloured pencil?

Black instead of a "lead"?

Good question @Babs.  I don't know.  Thinking it was  a "normal" pencil, not a colouring one.  I'll try to remember and take some pics on Wednesday,.  I'm sure some of the pots are still on the shelf at the centre.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.


×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.