i like printer's blankets.   they need to be sponged off after a day of use but it is easy because the fabric is so tightly woven.  they are wonderful and if you have an offset printer nearby they can be free.  you just need to clean off the ink from the rubber side.  mine are about 24 by 30 and  i have used them for years.  still look and act new.

Share this post


Link to post
Share on other sites

The old original slab mats had no texture on one side. After 15 years or so they got a little brittle. The new ones have a texture that I don't like but are much smoother than anything else. I use them for my large slabs for raku.

 

Marcia

 

Share this post


Link to post
Share on other sites

I bought a slew of slab mats long ago. I called and bought them as seconds and trimmed off the bad parts -they where very reasonable. I use one every week for over a decade and its still in good shape. They areall smooth on one side.My electric slab roller is 30 inch wide and 5 feet long so I got the large ones.I have a stailess rood that they hand from like a towel rod-all my matts hang on that.

Share this post


Link to post
Share on other sites

I love slab mats but make sure you get one for each colour of clay you use! I've made that mistake more than once... Also, if you don't let them dry out after a few uses, they can get "draggy" on your clay if using a slabroller, and one of mine has permanent wrinkles because I didn't listen to my instinct and pushed it for one more use :P

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.


×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.