13 hours ago, Tina E said:

Is it ok to mix mid-fire and low fire glazes on the same piece and fire at cone 04? What happens with the cone 6 glaze when it is fired at cone 04 temps? Thanks

My first pottery teacher's answer was "you can't"  when I pushed further she said "it won't work".  When I pushed even further she said "try it!"  I did. 

She and @neilestrick were right.  It doesn't work, but don't let us stop you trying! 

And if you're tempted to try the other way, ^04 glaze in a ^6 firing, be sure to use a large cookie/catcher under your pot to catch the over-melted glaze and slumped clay.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.