hello

I trying to use De air  pugmill to eliminate the air bubbles in my clay, that mixed from 2 local clays.

After 3 times pugging, it still inside the clay when it throw it on wheel.

but i 've checked by cutting into thin sheet thickness around 5mm. , there is no air bubbles there. 

 

Anyone have faced this problem, and how to solve it because now we have quite a lot stock for this clay.

Ps. I did some solutions like

- pug more 3,6,9 times

-wedge  more 300,600,1200 times/5kg.

- add some addition beer, vinegar

- let it dry 3-5days

but it's not work.

 

 

Thank you

Warm regards.

nguan 

 

  

Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.