oldlady Posted September 30, 2019 Report Share Posted September 30, 2019 just mixed my good clear glaze with robins egg for the first time. no idea of the exact color but i am afraid it might come out too close to the cerulean blue i already use by the look in the bucket. is it really a greenish blue or not? cannot find a color chart right now. i am looking for a middle sort of sky blue without green tones. anyone know a good mason stain to give me that? Link to comment Share on other sites More sharing options...
Pres Posted September 30, 2019 Report Share Posted September 30, 2019 What clay are you using it on oldlady? I have found that transparent glazes really react differently depending on clay color and use of base color, even when working on a white body with areas of white base glaze and bare areas the differences in value and hue can be quite dramatic. best, Pres Link to comment Share on other sites More sharing options...
oldlady Posted September 30, 2019 Author Report Share Posted September 30, 2019 white clay, little loafers from highwater, cone 6 electric. Link to comment Share on other sites More sharing options...
Joseph Fireborn Posted September 30, 2019 Report Share Posted September 30, 2019 oldlady robins egg is what i used for my faux celadon stuff a while back this is 1% if I remember right on standard 365 thin application: thick application: Link to comment Share on other sites More sharing options...
oldlady Posted September 30, 2019 Author Report Share Posted September 30, 2019 BEAUTIFUL!! THANK YOU, JOSEPH! Link to comment Share on other sites More sharing options...