Can a glaze expert answer this?  What are the crystals in those commercial glazes?  I want to experiment with my own, but I don't know where to begin.  After rinsing the crystals in the commercial glazes, they appear to be broken glass, but surely that's not it.  Can someone illuminate this for me?  I'm a novice at making my own glazes...  Thank you!

Link to post
Share on other sites

Neilestrick,  thanks for responding.  I found a post on here from someone that explains how to make the glaze chunks that you can use.  I'm definitely going to try this.  I also want to use the frit though.  HI've also seen posts on how to crush your own frit, but what kind of glass do I start with?  How do I find  glass/frit that will melt at the right temperature?  Most of my stuff is cone 06.  The only other mentions of trying to find the frit yourself is to "make sure the frit you use melts at the right temperature".  At which point in the firing process is the frit supposed to melt?  

 

I really appreciate your responses!!

Link to post
Share on other sites
12 hours ago, skessel1 said:

HI've also seen posts on how to crush your own frit, but what kind of glass do I start with?  How do I find  glass/frit that will melt at the right temperature?  Most of my stuff is cone 06. 

Is this the effect you are looking for? Amaco low fire "crystals" to either sprinkle on wet glaze or stir into the wet glaze. 

image.png.d192d3fa68c941dc4d6c679bcaabfd00.png

Link to post
Share on other sites

Hi Min,

 

I've seen those Amaco ones.  But, $25 for 4 oz!!!  No way.  I'm hoping to make my own, I'm just not sure where to begin.  I'd really like to add glass, but I'd like to know what kind of glass chips I need.  I have washed the "crystals" from the duncan commercial glazes and they are indeed crushed glass... but not all glass is the same I'm sure...  Just hoping someone could throw me some pointers to get me started.  Thank you!

Link to post
Share on other sites
5 hours ago, skessel1 said:

I'd really like to add glass, but I'd like to know what kind of glass chips I need.  I have washed the "crystals" from the duncan commercial glazes and they are indeed crushed glass... but not all glass is the same I'm sure... 

I don't think the Amaco "crystals" are just your basic soda lime glass frits. I haven't seen recipes for the Amaco type crystals but I would imagine they would be made from low fire glazes with colourants. Making your own and getting them to melt just enough would take some testing. I think you could actually forgo the fritting part of the process if you dried the glaze out and  broke it apart into little chunks. The little bits would need to be placed on the wet base glaze and obviously not mixed into it.

The topic of melting glass onto pots has come up many times on the forums, one thread that I started is here. General consensus is it's not a good idea.

Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.