A once fire is a bisque and then a glaze fire.  If you had a kiln load of once fire, you might duplicate the bisque schedule for the first 400 at least.  The only  real trick to once fire is the glaze application on greenware.  If you're only wanting to see the body, no glaze, go for it.  Be sure to run some shrinkage measurements.  Personally, I'd be bisque firing a bunch of test tiles if I wanted a new porcelain body (especially)

Link to post
Share on other sites

I should have said A once fire is a bisque and then a glaze fire ALL IN ONE FIRE.  What I was trying to say was that a single fire (once fire) goes through the bisque process and then continues on to glaze temps.  Doing a glaze fire with all bisqued pieces isn't doing much below the highest bisque temperature except burning off glaze water, wax etc.  You don't have to run bisque speeds.  A single fire needs to run bisque temperature ramps.

Link to post
Share on other sites

@CactusPotsThank you for your input Getting  back to shrinkage Clay shrinks whilst drying Shrinks in one firing & bisque firing Is there more shrinkage at the glaze phase ? Trying to figure out shrinkages Just opened kiln happy with results ...... aside from shrinkage 

Thank you Nicky 

 

Edited by Nicky S
Link to post
Share on other sites

Each phase of drying has shrinkage.  I know because of disasters I have had from each.  Mostly concerning larger pots.

To go to bone dry, I use a piece of newsprint under the larger pots to facilitate movement.

To bisque, I use a thin layer of grog under foot.

In a glaze fire, I use little blocks of soft brick under the feet, for runny glazes.  If the foot of the pot is too close to the inside edge of the soft brick pad, it can walk right off.

Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.