They are all prone to clouding if they're applied too thick. But Tony Hanson put this out in the last few weeks. It’s the summation of all the testing he’s been doing to find a fluid clear. 

https://insight-live.com/insight/share.php?z=gbcM8HXmX2

 

Edited to add:

He’s got some images of his latest recipe over Plainsman’s new black clay, which has given all my glazes bubbles so far. It looks pretty crystal to me. 

Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.