Hi,

I’ve been working with gold lustre and recently changed brands.  I’m  familiar with that dreaded purple that appears when the lustre is too thin, and I’ve also seen the lustre crackle when it’s too thick. I’ve not seen this matte kind of finish which is in the photo attached. The piece was glazed entirely and shiny before application. 

Is the application too thick or thin?

If I reapply and refire will it go shiny gold?

or is there something else wrong?

:(

534BDEA9-C979-42BA-838B-09A876A724A6.jpeg

Share this post


Link to post
Share on other sites

It's a little hard to tell from the pic, but it doesn't really look like what I would call a "matte" finish - at-least not on the gold.  To me, it looks like it's a shiny finish that's not on a perfectly smooth surface. 

Looks to me like the whole piece has a bit of an orange-peel texture to it, and looks like there may be some bubbles in the clear around the base of the raised area with the lustre on it.  I think the lustre is just amplifying the underlying surface texture. 

 

Share this post


Link to post
Share on other sites

Great thing about gold lustre is that you never have to guess what it will look like.  It will look EXACTLY like whatever you put it over, only gold.  It'll never smooth anything or change texture, because it is a layer of gold a micron or two thick. 

Your glaze is very bubbly, so the lustre looks like it's covering bubbles.

Edited by liambesaw

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.