Smoothing Uneven Surface On Greenware

Recommended Posts

I trimmed some pots that were slightly unevenly dry, and now the outside surface is unevenly textured. They're smooth in spots, but groggy and gritty in others. Is there anything I can do at the greenware stage to homogenize the surface?

Share this post


Link to post
Share on other sites

If your wheel is reversible, take a second or two to recenter, and using the wheel in reverse use a rounded wooden spoon or other tool to smooth/burnish.

 

 

best,

Pres

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.