On 10/10/2019 at 4:26 PM, Stephen said:

The one problem I have with the sheetrock though is that stacking them right after mold release will result in my tiles being flattened to bigger dimensions and resulting thickness reduced.

Have you tried using spacers between each sheet?

Share this post


Link to post
Share on other sites

I dry my large slabs between sheetrock boards lined with newsprint. I get end rolls from the local newspaper and have it on a gift wrap paper dispenser. I also was the edges as someone mentioned earlier that edges drying out first can cause warping.

Marcia

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.


×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.