Wingnut Posted May 21, 2019 Report Share Posted May 21, 2019 Bisquing at 04. Kiln sitter switched off. Witness cone still erect. Low fire on slow setting. Small kiln not filled. Should i manually continue to fire until witness cone bends? TIA. Jane Link to comment Share on other sites More sharing options...
Wingnut Posted May 21, 2019 Author Report Share Posted May 21, 2019 More info: it's been firing for about 8 hours. Link to comment Share on other sites More sharing options...
liambesaw Posted May 21, 2019 Report Share Posted May 21, 2019 Yes, wait for the cones, maybe the kilnsitter cone broke. Link to comment Share on other sites More sharing options...
Wingnut Posted May 22, 2019 Author Report Share Posted May 22, 2019 Thanks for quick reply! I fired manually for about another 1 1/2 hours before cone bent. Can't wait to see it in the morning after it cools. Link to comment Share on other sites More sharing options...
neilestrick Posted May 23, 2019 Report Share Posted May 23, 2019 Could be a broken cone, or your sitter is not calibrated. Link to comment Share on other sites More sharing options...