:oOh well, once again, we seem to be lacking suggestions for the QotW.   I will humbly submit another of my own, with the catchy tongue in cheek phrase. . . Does size matter?  Now that we have your attention, I will clarify.  Recently I saw one of the most derided (by potters) movie representations . . . from Ghost , In the scene Demi Moore is throwing a large vase. . . sensuously. Whoa, but wait. . . is that piece being thrown off the hump? Why would they do that? Size! 

So that got me to thinking, about my own use of the hump, and throwing and how I use throwing off the hump. Most times I would never throw a vase of size off the hump unless there were something special about the trimming, or the some other structural thing involving the form. Most of my throwing off the hump would be smaller items like cups, mugs, chalice stems, lids, and other things that I can reasonably repeat the shape and  size by using my hands and relative ball sizes to repeat the same form over an over.

That got me to thinking about size in slabs also. . . especially when using a slab roller. I usually would roll out the largest slab I could, and cut pieces from that slab to build with. Often using a template, but many times using multiple smaller pieces to assemble without a template, only a sketch or mental idea of what I wanted to do, like a castle on a rugged mountaintop all out of slabs. The size of the slab did matter, as I often used edges, and other areas when needed, then used large pieces for base and interior  supports.

 

So in you work, Does size matter? Why, How, When!

 

best,

Pres

Link to post
Share on other sites

The thing about size for me, is that I find it annoying to center anything from about a pound and under.  15lbs? No problem, 12 ounces? Why bother.    So if I am going to do some smaller items I will throw off the hump just because it's so hard for my big hands to center anything that small.  For mugs and bowls I'll do chunks of 1lb, still takes a minute to center sometimes.  I do love making a nice big pot though, something alluring in making something that big even though it's useful for nothing.

Link to post
Share on other sites

i think that once i can make something in any size i want, i am satisfied that i have learned that skill and can go back to the normal size for me.  yes, i can make a huge salad bowl for 20 people but would rather make 20 personal size salad bowls.

Link to post
Share on other sites

In my 35 forms they vary from larger cannistyers to 20# large bowls to 1/2# spoonrests.

Size maters depending on the form.

For me right now the real income is in small stuff-like the 120 spongeholders I sold to one outlet-they pay the bills.

Yes I can make the big sectional pots but I'd rather make lots of meduim bowls.I sell about 2-3 a week in my outlets where a large pots sit for 1/2 a season .

Edited by Mark C.
Link to post
Share on other sites
8 hours ago, Pres said:

 

That got me to thinking about size in slabs also. . . especially when using a slab roller. I usually would roll out the largest slab I could, and cut pieces from that slab to build with.

So in you work, Does size matter? Why, How, When!

 

best,

Pres

When rolling slabs, the advice I read from Alfred Ceramics, is to cut from the centre of a larger slab, to eliminate the weird stretching that happens around the sides.  http://www.readypedalgo.co.uk/Particles-%20Orientation%20and%20Density%20-%20Alfred's%20Clay%20Store.pdf, page 55

So, yes, size does matter.

Link to post
Share on other sites

I do some large pieces, some fully thrown, some with wheel thrown and slab elements combined. Check my albums. Combining forms takes considerably less energy, but design becomes even more important as proportion, texture, and details become more important when combining in that manner.

 

best,

Pres

Link to post
Share on other sites
  • Pres unpinned this topic

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.