Demi Posted April 15, 2019 Report Share Posted April 15, 2019 I need a programme for firing from 0 degrees up to 1260 degrees approx for a Y material piece. NO glaze involved. I've done this successfully before but am never sure precisely what I've done ( not being very scientific ! ), so would like some input and suggestions. thanks ! Link to comment Share on other sites More sharing options...
Min Posted April 15, 2019 Report Share Posted April 15, 2019 Hi Demi and welcome to the forum! What is the size of the piece you want to fire, how thick and how dry is it? I'm assuming you are using celsius and going from room temp not frozen? What type of kiln do you have, manual where you turn the dials up or a computer controller on it? Link to comment Share on other sites More sharing options...