Accidental 15 hour hold at the top of a bisque


Recommended Posts

How can your hold be for so long...accidentally

Try to log your firings get in your hesd or on papercapprox time your firings take and set an alarm somewhere.

Better still get a timecattached to your kiln which will shut off about 30mins after your estimated firing should finish.

Dont walk away, computers do fail but most errors are human.

Sorry but a bitvshocked at leaving kiln on 15hrs after reaching desired temp...

Hope everything works out but if not...steep learning kiln.

U can flick through what you've programmed before starting your firing.

A good practice imo.

 

Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.