As I am limited in building big pots because of the kiln size, I am considering to use frost resistant concrete for the larger objects. Is there a concrete that will act like clay? The internet is full of articles regarding ShapeCrete but it is not shipped to Europe and it doesn't seem to be like clay.

How is this made out of concrete? WIth an armature mesh? 

2019-03-24 17_56_43-Window.png

Share this post


Link to post
Share on other sites

@VladCruceanu

There is an admixture for regular concrete to increase the PSI; used mostly to make concrete countertops. You can add  colorants, aggregates, etc.  Google search: " concrete countertops."  It will get you into the products you need. Here is an ebay link for admixture:

https://www.amazon.com/Concrete-Exchange-Countertop-Kit/dp/B01L2SRAA6/ref=asc_df_B01L2SRAA6/?tag=hyprod-20&linkCode=df0&hvadid=242015060393&hvpos=1o4&hvnetw=g&hvrand=3306324636649431258&hvpone=&hvptwo=&hvqmt=&hvdev=t&hvdvcmdl=&hvlocint=&hvlocphy=1016434&hvtargid=pla-644100411970&psc=1

Tom

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.