Hello.

I have a few high-fired glazed pieces that I'm unhappy about. Is it possible to re-glaze using earthenware glazes and then re-fire at earthenware temperatures? The reason for doing this is simply so I don't have to fire at such a high temperature again (trying to reduce time and cost)

So just to clarify: would a low-fire glaze work on top of a previously fired high-fired glaze?

Thank you.

Edited by Momo
Link to post
Share on other sites
25 minutes ago, Momo said:

Thank you. Yes, I thought I'd give it a try anyway but just thought I'd ask as I'm guessing I'm not the first person to want to try this. 

Yeah, the problem with a question like this is that the answer will always be "it depends", just because of all of the variables involved.  It's been done millions of times but each time and situation is a little (or a lot!) Different so the likelihood of one persons experience translating to your situation is probably unlikely.

If it works let us know, and then keep track of it for yourself too. You'll know that x glaze over y fired glaze = success or failure, and you can use that knowledge next time you want to reglaze

Link to post
Share on other sites
10 minutes ago, liambesaw said:

Yeah, the problem with a question like this is that the answer will always be "it depends", just because of all of the variables involved.  It's been done millions of times but each time and situation is a little (or a lot!) Different so the likelihood of one persons experience translating to your situation is probably unlikely.

If it works let us know, and then keep track of it for yourself too. You'll know that x glaze over y fired glaze = success or failure, and you can use that knowledge next time you want to reglaze

Good advice. I'll let you know how I get on.  Thanks again. 

Link to post
Share on other sites

I’ve done it many times with mostly positive results, the difficulty is getting a sufficient enough layer of new glaze material to stick to the previously glazed vetrified piece. I’ve never used hair spray although have read it can help the glaze to adheare, if the piece is small enough I’ll put it in the microwave for a minute or two that will do 2 things , heat the surface a little and neutralize some of the surface oil from things like oil transferred from skin contact. Otherwise I’ll heat it with an electric heat gun, Then  work quickly while the piece is warm.  Use a loaded brush, a soft touch and try to avoid going over areas a second time as repeated brush strokes will begin to work against you. You will have to practice a little to get the feel, luckily if it fails to apply like you like it’s very easy to rinse off the newly applied glaze and start over.

Link to post
Share on other sites
52 minutes ago, 1515art said:

I’ve done it many times with mostly positive results, the difficulty is getting a sufficient enough layer of new glaze material to stick to the previously glazed vetrified piece. I’ve never used hair spray although have read it can help the glaze to adheare, if the piece is small enough I’ll put it in the microwave for a minute or two that will do 2 things , heat the surface a little and neutralize some of the surface oil from things like oil transferred from skin contact. Otherwise I’ll heat it with an electric heat gun, Then  work quickly while the piece is warm.  Use a loaded brush, a soft touch and try to avoid going over areas a second time as repeated brush strokes will begin to work against you. You will have to practice a little to get the feel, luckily if it fails to apply like you like it’s very easy to rinse off the newly applied glaze and start over.

Thank you!

Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.