Hi Alice,

I've glued 6" diamond wheel to a bat (my least favorite bat, which can still be used for clay, flipped over...) for polishing feet - works great! I run the wheel at a moderate speed, wet. The sludge (wet dust) likely wouldn't change how my clay behaves - I'm cleaning up before and after anyway.

A courser grit would probably be better; this was so inexpensive tho'

 

dd.JPG

Share this post


Link to post
Share on other sites

I really like the idea of grinding wet to eliminate dust issues, I’ll have to pick up a suitable diamond abrasive wheel, I’ve glued wet sanding disks to old throwing bats but their useful life is short. I did lapidary work many years ago and we used a flat lap that didn’t seem much different than a wheel head with a 1” lip to dress the backside of polished stones a much more involved version of Hulks method. 

Sometimes I’ll chuck a finished piece on my giffen grip and hang a bag of water over the wheel head to provide a steady drip of water then use a diamond burr while spinning the ceramic ware on the wheel. Not the easiest way to go about finishing the bottoms, but if I’m not in production mode I’ve saved a few glaze disasters and am able to produce very clean edges with glazes that like/need to run and have smoothed bottoms with it.

Edited by 1515art

Share this post


Link to post
Share on other sites

"...steady drip of water then use a diamond burr while spinning the ceramic ware on the wheel." 

Good idea! 

Regarding the diamond wheel glued to an old bat, I went with 1200 grit because it was cheap and for sure would leave a polished surface. However, it is a bit slow - a 600 is probably fine enough to get a nice polish, and would be faster. Back to the other hand, 1200 is forgiving and doesn't "grab" much. 

Share this post


Link to post
Share on other sites

I have used the following techniques to make the bottoms of coarse clay body items smoother.  They all work, some better than the others.  For really coarse clay bodies, the combination of 1, 2, and 6 are what I try to remember to do. 
Random order of use:

1. burnish the contact area at the stiff leather hard stage.
2. apply terra sig to the contact area at bone dry stage and burnish.
3. smooth the bisque ware contact area using fine emery paper taped to a smooth surface, or with a medium and then fine grain sharpening brick. 
4. fine emery paper (~200+ grade) glued to a bat on the wheel. use wet.
5. polish glazed fired items with emery sharpening brick.
6. polish glazed fired items with a medium to fine flap wheel on a grinder or drill press.

Diamond wheels are OK, but are overly expensive, in my opinion, for most items unless the sales price of the final ware item covers the cost of the diamonds. 

LT

 

Share this post


Link to post
Share on other sites
40 minutes ago, Hulk said:

"...steady drip of water then use a diamond burr while spinning the ceramic ware on the wheel." 

Good idea! 

Regarding the diamond wheel glued to an old bat, I went with 1200 grit because it was cheap and for sure would leave a polished surface. However, it is a bit slow - a 600 is probably fine enough to get a nice polish, and would be faster. Back to the other hand, 1200 is forgiving and doesn't "grab" much. 

Specifically, I use an old camel,back bladder it has the bag (naturally), hose,  valve, a hook to hang  and a snip of the mouthpiece with a diagonal cutter makes the nozzle. Holds plenty of water and you have great control over the drip. If you have access to medical supplies an iv drip works too.

Edited by 1515art

Share this post


Link to post
Share on other sites
7 hours ago, Magnolia Mud Research said:

I have used the following techniques to make the bottoms of coarse clay body items smoother.  They all work, some better than the others.  For really coarse clay bodies, the combination of 1, 2, and 6 are what I try to remember to do. 
Random order of use:

1. burnish the contact area at the stiff leather hard stage.
2. apply terra sig to the contact area at bone dry stage and burnish.
3. smooth the bisque ware contact area using fine emery paper taped to a smooth surface, or with a medium and then fine grain sharpening brick. 
4. fine emery paper (~200+ grade) glued to a bat on the wheel. use wet.
5. polish glazed fired items with emery sharpening brick.
6. polish glazed fired items with a medium to fine flap wheel on a grinder or drill press.

Diamond wheels are OK, but are overly expensive, in my opinion, for most items unless the sales price of the final ware item covers the cost of the diamonds. 

LT

 

Wonderful thank you! 

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.