On ‎1‎/‎19‎/‎2019 at 5:48 PM, glazenerd said:

Jim:

i have used Miniwax Finishing wax for many years on wood: it dries clear satin. Do not know how it would act on ceramic; but it should retain its clear finish. Test it, is all I can advise.

T

We have used this product as well on pit and saggar pots, it works well.  It can be buffed to high shine or left more satin.  It does have a slight yellow tinge to the final product especially if it is a thick application.

Share this post


Link to post
Share on other sites

I too use the Future acrylic floor wax, now branded as Pledge Floor Care Finish. As nobody has linoleum floors that need to be waxed anymore, most stores selling household care products don't carry it, so I now order it online from the big river in South America. I apply 2 light coats with a foam sponge, and you can handle it very soon after applying the wax. Straight from the bottle, it will be pretty glossy, but I've found I can reduce the gloss somewhat by cutting the wax half and half with water.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.