Wayne H. 4 Report post Posted December 8, 2018 Can I use a brushing glaze over a dipping glaze , both are Amazon glazes? Quote Share this post Link to post Share on other sites
Wayne H. 4 Report post Posted December 8, 2018 A correction, they are Amaco Glazes not amazon. Sorry I have Amazon on the brain. 1 Rae Reich reacted to this Quote Share this post Link to post Share on other sites
Dick White 301 Report post Posted December 8, 2018 That can be done. The glazes should be of compatible firing range. The exact outcome of the combination will be unknown until you test it. 1 Roberta12 reacted to this Quote Share this post Link to post Share on other sites
JohnnyK 463 Report post Posted December 9, 2018 Amaco promotes the layering of many of their glazes with a variety of outcomes. I have been using their Potters Choice line with great success for a number of years now (see the latest addition to my album). All of the work that I do is brushing which can be very tedious and I have considered the dipping then brushing aspect because much of my work is a variable second color over a solid first color. I don't see any reason why you couldn't brush a second or third glaze over a dipped first color and would suggest that you do a few tests to find out what happens... some small bowls or even broken pots would give you a better idea of the glaze fx than test tiles. JohnnyK Quote Share this post Link to post Share on other sites
neilestrick 3,330 Report post Posted December 9, 2018 Glazes that are mixed from dry materials are not very durable for brushing on top of. Brushing glazes have binders and hardeners that not only make them flow better with a brush, but hardens the surface so it can be brushed over with another layer. Dipping glazes are quite soft and fragile by comparison, especially those that are lower in clay content. You may find that brushing on top of a dipping glaze just ruins the dipped layer. If your dipped layer is a commercial glaze that was purchased as a wet glaze, then it is most likely a brushing mix, even though you dipped it, and it will be fine for brushing over. Quote Share this post Link to post Share on other sites
Pres 1,913 Report post Posted December 9, 2018 As Neil has said, wet commercial glazes are made for brushing unless you are buying from a glaze formulator you have contracted for a glaze formula you have. Amaco being a commercial manufacturer tries to make all of their glazes in a series compatible with one another. I have had problems dipping Amaco straight from the container so would water them to a chocolate milk consistency. Then I would apply any brushed areas overtop with the straight from the jar glazes. best, Pres 1 Rae Reich reacted to this Quote Share this post Link to post Share on other sites