Bisque firing to cone 06 instead of 04 will leave the pots slightly more porous, so if you're dipping to apply glaze, you won't need to dip as long. Other than that it shouldn't cause any problems unless you're using a dark stoneware where all the organic stuff isn't getting burned out completely by 06.