Sorry for the repost - I realized it belongs in this section.

-----------------------------------------------------------------------

 

 

Hello! I create layered wall plaques (like layed tiles) and I am having serious crack problems. At first, I was only having cracks in these pieces in the glaze kiln, but now I am getting cracks in the bisque kiln as well. I have tried several solutions suggested to me, but the problem still exists. The cracks are in the bottom of the pieces (side touching shelf) and sometimes will come through to the front of the piece. They mainly begin at the top of the piece and go towards the center, but not always. Some cracks are very slight, and some are pretty deep and wide.

 

Please advise... I have boxes of plaques with cracks and it is very disheartening to loose so many pieces.

 

Thank you!!

 

Malena

Share this post


Link to post
Share on other sites

Hello Malena

Might the cracking be due to parts of the tiles sticking to the kiln shelf during firing? Maybe try an extra coating of bat wash on your shelf so the tiles can shrink without encountering any resistance. Your work sounds very interesting ... any pictures?

Kind regards

Christine

Share this post


Link to post
Share on other sites

Hello Malena

Might the cracking be due to parts of the tiles sticking to the kiln shelf during firing? Maybe try an extra coating of bat wash on your shelf so the tiles can shrink without encountering any resistance. Your work sounds very interesting ... any pictures?

Kind regards

Christine

 

 

 

Hi Christine,

 

Thank you for the suggestion - I appreciate it. I have some pictures on my website: www.mbwclayartist.com - thanks for your interest!

 

Malena

Share this post


Link to post
Share on other sites

Sorry for the repost - I realized it belongs in this section.

-----------------------------------------------------------------------

 

 

Hello! I create layered wall plaques (like layed tiles) and I am having serious crack problems. At first, I was only having cracks in these pieces in the glaze kiln, but now I am getting cracks in the bisque kiln as well. I have tried several solutions suggested to me, but the problem still exists. The cracks are in the bottom of the pieces (side touching shelf) and sometimes will come through to the front of the piece. They mainly begin at the top of the piece and go towards the center, but not always. Some cracks are very slight, and some are pretty deep and wide.

 

Please advise... I have boxes of plaques with cracks and it is very disheartening to loose so many pieces.

 

Thank you!!

 

Malena

 

 

Malena, I visited your website and your work is utterly charming. I'm intrigued by the almost black stain (?) that gives dimension to your underglazed (??) finishes. I'm a newbie to underglazes and glazes, and I'm trying to find something that will give me that slightly aged appearance. Would you be willing to share your technique for finishing?

Thanks, Jayne

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.