I have a frit that I can not find a substitute for. I have also never understood unity formulas as well. I'm hoping someone cal help translate this back to raw materials

The frit number is 1290 it has only 4 components  NaO .50  Cao .50  B2O3 1.00 and silica 2.oo

Am I guessing correctly that 1 part borax i part whiting and 2 parts silica would be some thing close to the frit or is there a better set of ingredients to use

Thanks

 

Share this post


Link to post
Share on other sites

Great,

1290                                      16.36%     The frit number is 1290 it has only 4 components  NaO .50  Cao .50  B2O3 1.00 and silica 2.00

Custer feldspar                  18.39

Dolomite                               17.55

whiting                                      2.50

EPK                                          16.85

Silica                                         23.95

Titanium Dioxide                    3.42

Cobalt oxide                                .74

Iron Ox                                          .02

NiO                                                 .28

It's a variation of float blue I'd like to test. The frit has thrown me off as could not find a substitute

Thanks for any help Wyndham

 

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.