I had a collaborative project with a friend.  I made the trays, she applied the black underglaze and did the sgraffito work.  I bisqued the pieces to 04 and sprayed them with clear.  All of the pieces came out with a white speckling and slight pitting.  I have not noticed this effect on my other work with underglaze and clear.  But I do not normally use large expanses of black.  Does anyone have any thoughts or suggestions?  We would love to do more of this work. 

Roberta

IMG_20170926_104014512 sgraffito.jpg

Share this post


Link to post
Share on other sites

Looks like boron clouding in the whitish/blueish areas. Is the glaze thicker in those areas? Pitting can be from a few things. How clean was your bisque fire, were the pieces stacked in the bisque, vented or not? Could also just need a hold at the top temp to smooth the glaze over. Sometimes it's from overfiring. Since the pieces are all shallow and flat I would look at the possibility of them just not getting hot enough at the end of the glaze fire. I have a low coe clear that works well over black (Spectrum) ug if you want the recipe just let me know and I'll pm it to you.

Share this post


Link to post
Share on other sites
On 10/8/2017 at 9:33 PM, dangerouspottery said:

Min, I would love the have the recipe for that clear glaze that works over underglaze, if you don't mind.

Thank you!

Did you get the PM with the recipes I sent yesterday?

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.