ppony123 1 Report post Posted June 23, 2017 THANKS for the suggestions for reading some of the Hopper books. I finally got one. I look forward to getting a few more. I discovered this technique I've always liked but never new what it was called so I've been trying to emulate it for the past few weeks. Cuerda seca. I found a recipe on a site for making my own black wax to use for the lines which was just some black stain in emulsified wax resist, but following it and then after firing, the black just came off as if like dry charcoal. I fired on ^04 earthenware bisque to ^05 ramping up at 200 per hour. What did I do wrong? the recipe called for the resist to be of a paste consistency but I can't help but think that contributed to the lack of adhesion. It's so hard to find information on this technique. Especially in english. I'm going to be firing few tests tonight of the wax resist at a few different thinner viscosities. But I was hoping that I might gain some insight from your brains. THANK YOU!! Quote Share this post Link to post Share on other sites
Min 2,267 Report post Posted June 24, 2017 The black stain isn't going to stick to the pots by itself. You need to add some frit or gerstley borate or what would probably work better would be to just use some dry black glaze, one you know doesn't move during firing, and mix that with your wax resist. The original Cuerda Seca used manganese which will fuse to the clay but not a good thing to use health-wise. Would love to see what you do with it! Quote Share this post Link to post Share on other sites
ppony123 1 Report post Posted June 24, 2017 The black stain isn't going to stick to the pots by itself. You need to add some frit or gerstley borate or what would probably work better would be to just use some dry black glaze, one you know doesn't move during firing, and mix that with your wax resist. The original Cuerda Seca used manganese which will fuse to the clay but not a good thing to use health-wise. Would love to see what you do with it! Thanks, Min! Yeah, that was something I was wondering. It seemed odd that it said it was going melt into the clay on its own w/o something to actually melt. I'll add some frit. Stay tuned! Quote Share this post Link to post Share on other sites
alabama 154 Report post Posted June 24, 2017 Is there an example of what you're trying to accomplish, on this cuerda seca du jour? Alabama Quote Share this post Link to post Share on other sites
Mark (Marko) Madrazo 178 Report post Posted June 24, 2017 There is a mix made for this called Artistic Line Resist. www.artisticceramics.net 626-968-8661 Best wishes. And share your journey. Quote Share this post Link to post Share on other sites
Marcia Selsor 1,783 Report post Posted June 24, 2017 As mentioned above the pigment/metal oxide needs a little flux like frit 3134. The technique is old and was revived in the tile industry in the Romantic California period around the 20s.(1920s). The Big ceramics store sells the premixed wax. The original Spanish recipe calls for an oil from a certain tree in Spain, "Balsano de Copiano". I still have a bottle of it from when I did my research there in 1980s on my Fulbright. I visited the city of Cuenca and potters in rural areas in the Province of Cuenca. Here is the info on it from the Big ceramic Store. http://www.bigceramicstore.com/info/ceramics/tips/tip74_cuerda_seca.html Stephani Stevenson gave the talk on it at NCECA when we presented a dual lecture on Architectural Ceramics from Central Asia to Hollywood in Louisville. She showed some stunning installations from tile companies like Capri Tiles from the 20s. Marcia Quote Share this post Link to post Share on other sites
douglas 29 Report post Posted June 27, 2017 THANKS for the suggestions for reading some of the Hopper books. I finally got one. I look forward to getting a few more. ... found a recipe on a site for making my own black wax to use for the lines which was just some black stain in emulsified wax resist, but following it and then after firing, the black just came off as if like dry charcoal. Post the recipe if you want help on how to fix this. Pictures make it easier for people to help you too. Quote Share this post Link to post Share on other sites
ppony123 1 Report post Posted July 8, 2017 THANKS for the suggestions for reading some of the Hopper books. I finally got one. I look forward to getting a few more. ... found a recipe on a site for making my own black wax to use for the lines which was just some black stain in emulsified wax resist, but following it and then after firing, the black just came off as if like dry charcoal. Post the recipe if you want help on how to fix this. Pictures make it easier for people to help you too. I think the problem was that they suggested using reclaimed dry glaze OR stain. They just went on the assumption that everyone would use the glaze that already had flux and people would know to add flux if they were just using stain. So, my bad, of course. I did a bunch of tests and finally got it to where I had added enough flux that it fused and didn't come off. I would have liked to have posted pix of what I was looking to do, but I can't seem to get pictures to load. Sigh THANKS so much! So much to learn and so many failures just get so frustrating. Quote Share this post Link to post Share on other sites
Jennifer L. 1 Report post Posted November 2 Take a look at this thesis I found online “CUERDA SECA CERAMIC TILES: EXPLORATIONS OF RESIST FORMULAS IN VARIOUS FIRING RANGES by Carla Aubin Sotelo” It has a vey in depth (91 pages!) look at different materials the author tested for resist formulas. 1 Magnolia Mud Research reacted to this Quote Share this post Link to post Share on other sites
Babs 899 Report post Posted November 2 Maybe that info should go into topsectiin topics so it wont be lost. Quite a few folk have had queries re. Cuerda seca Quote Share this post Link to post Share on other sites