So I have been using my woodburner like crazy and instead of tossing my ashes out I have been saving it. Its amazing how quick the ash pile grows and I would like to make some glaze with it.

 

Was wondering if anyone has any good glaze recipes requiring a large amount of wood ash. Pictures of the glaze after would be great if possible.

Share this post


Link to post
Share on other sites

http://ceramicartsda...n-or-reduction/

 

This URL will get you one to start with and a couple of colorant subs to try. Also has a picture and fires to Cone 6, oxidation or reduction. I expect if you are looking for tan or brown you could try subbing in red iron oxide in the 2 to 5 % range to see the color response and include some test tiles with your next firing.

 

John

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.