1 hour ago, Marcia Selsor said:

This is what I use...adapted from Peggy Heer's  . 

 1:4 toilet paper to clay?  Soak toilet paper overnight, squeeze dry, add to dry clay, the same body as you are repairing..  Then add vinegar and a few drops of sodium silicate and mix with blender. I have repaired students' work with this as well as a sculpture of my own.\

Well if the new one cracks I'll try this, hopefully I won't need to.

Share this post


Link to post
Share on other sites
8 hours ago, pizzuti_ said:

Well if the new one cracks I'll try this, hopefully I won't need to.

Nooooooooooooo! Don’t accept cracks as the norm.  Unless you are going for cracks!

do something to prevent cracks - change claybody, how you make wares, Firing cycle - something so that cracks is a thing of the past. 

In our school we candle at 200 for 48 hours to avoid blowups and cracks. Thick pieces could be .5 to 1 inch thick.  I have been known to cook functional ware at the lowest setting in my home oven and had 6 pieces come out bone dry in 8 hours. Hand built.  Winter. No rain.  At a different school where kiln space was limited and the proff would only fire bone dry.  

Share this post


Link to post
Share on other sites
6 hours ago, preeta said:

Nooooooooooooo! Don’t accept cracks as the norm.  Unless you are going for cracks!

do something to prevent cracks - change claybody, how you make wares, Firing cycle - something so that cracks is a thing of the past. 

In our school we candle at 200 for 48 hours to avoid blowups and cracks. Thick pieces could be .5 to 1 inch thick.  I have been known to cook functional ware at the lowest setting in my home oven and had 6 pieces come out bone dry in 8 hours. Hand built.  Winter. No rain.  At a different school where kiln space was limited and the proff would only fire bone dry.  

I am not accepting cracks as the norm. I have a piece that I hand built in the dove porcelain, it's drying now and it's past leather hard, if it cracks, it cracks.  I'll let it dry a few weeks more then I will candle for a few days before I fire it. I'm not sure the issue with this piece was the firing. I don't think I built, or dried, it properly, I think the base stayed too wet. I did it differently on this one and I'm optimistic, we'll see.

Share this post


Link to post
Share on other sites
6 hours ago, pizzuti_ said:

I am not accepting cracks as the norm. I did it differently on this one and I'm optimistic, we'll see.

Whew! Good!!

its this we’ll see that keeps me going in ceramics.  I secretly think my favourite thing about ceramics is all the myriad of problems I have to solve!  And the even more fun part is actually predicting the problem and waiting to see it happens because then it proved your point.  

Share this post


Link to post
Share on other sites

Your base may be thinner than rest if not solid

You may be leaving moisture in pot

Get it off its base asap if not before.

Clay may not be wedged compressed enough in that area.

Research cracking...it's happened before.

Not wikip.

Share this post


Link to post
Share on other sites
20 hours ago, preeta said:

Whew! Good!!

its this we’ll see that keeps me going in ceramics.  I secretly think my favourite thing about ceramics is all the myriad of problems I have to solve!  And the even more fun part is actually predicting the problem and waiting to see it happens because then it proved your point.  

Ha, I really like repairing things.  I think I'd be perfectly content just doing restoration work :)

 

Share this post


Link to post
Share on other sites
18 hours ago, Babs said:

Your base may be thinner than rest if not solid

You may be leaving moisture in pot

Get it off its base asap if not before.

Clay may not be wedged compressed enough in that area.

Research cracking...it's happened before.

Not wikip.

Yeah, I did this time, I have it upside down on a screen to dry, fingers crossed....

Share this post


Link to post
Share on other sites
9 hours ago, pizzuti_ said:

Ha, I really like repairing things.  I think I'd be perfectly content just doing restoration work :)

 

Darn Pizzuti you missed your calling. An archeologist or museum restorer (sound boring but I’d give anything to hold the really old pieces) or a famous  kintsugi restorer in Japan. 

Edited by preeta

Share this post


Link to post
Share on other sites
1 hour ago, preeta said:

Darn Pizzuti you missed your calling. An archeologist or museum restorer (sound boring but I’d give anything to hold the really old pieces) or a famous  kintsugi restorer in Japan. 

Boring??? Sounds VERY exciting to me.  I might have to look into it....

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.