There is one shelf where the kiln wash flakes off every time it is newly applied. The other shelves, where the kiln wash is applied the same way, do not have this problem. Any suggestions?

Share this post


Link to post
Share on other sites

if you have a wire brush disc for a drill, that won't dig into the shelf and may remove whatever the problem is.

Either method will create a lot of silica dust. Wear safety googles and good dust mask. You may also want to wear a hat.

Marcia

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.