Kiln Shut Off Too Early - Can I Refire These Pots?


Recommended Posts

Hi - I was doing a glaze fire to cone 5 last night, and due to a dumb mistake on my part, the kiln shut off an hour too early.  My question is this: can I save these pots by refiring them to the correct temperature?  Can I do this without reglazing them?  Is it even worth it?  Any advice would be appreciated!  Thanks!

Link to post
Share on other sites
  • 1 year later...

Was this successful?   I have underfired a sculptural piece with matt glaze over underglazing bisqued.   Just come out looks like raw white glaze.    I would like to refire at the higher correct temperature, I had fired to 1080 C  and the glaze should be 1200-1280 C.      Appreciate any comments

Edited by AscotLady
Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.