Cone 6 Reduction Recipes From My Handouts

Recommended Posts

This is a handout from my last #6 Reduction workshop in Corpus Christi. This is a word document

Dan Engelke developed many ^6 reduction glazes at Lafayette University in the '70s and gave them out at an NCECA discussion group.I began working with ^6 reduction in 1980 when the ceramics lab was moved to a newer facility and the firings were supposed to fit into an 8 hours time slot. There is some repetition in this because of many pastings and adding.

^6recipes 2010 copy.pages.zip

^6recipes 2010 copy.pages.zip

Share this post


Link to post
Share on other sites

Thank you very much Marcia! I have only two years experience in this pottery making field so far but i really do love all aspects of it, especially the reduction glaze colors.  I have several reduction glaze recipes so far that i like, i am very exited to try some of yours!!

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.