On 5/27/2021 at 4:27 PM, liambesaw said:

Casting plaster is weaker now days, at work we switched from casting plaster to pottery plaster #1.  Much better quality and strength, and quicker setting time too!  

If you were casting a plaster wedging table, the thing to do would be to cast in a piece of expanded metal.  Used mostly for lath and plaster, I think, it's like chicken wire or hardware cloth, but more metal, less space.  Be like rebar in concrete on steroids.   My wedging table is still solid after 25 years and maybe 2" thick.  Well supported also.

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

 Share

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.