I have a wonderful aqua glaze that has been reliable for years but now pinholes consistently. I fire to 2185 w/a 30 min hold, slow cool in a Skutt electric. The recipe is:

Flint 26 Laguna Borate 22 Custer Feldspar 20 Frit P25 13 Neph Sy 9 Zinc Oxide 7 Talc 3   100 Add:   Copper Carb

2.5

 

Any ideas for why this is happening or how to fix it?

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.