Does Anyone Know How To Achieve Similar Results To This?

Recommended Posts

Welcome to the forum!

 

That looks like a variation of terra sigilatta combined with a carved surface ...

 

You can search this forum for many past discussions of terra sigilatta or go to the link on the top left of this page and find a lot of tutorials and videos on the Ceramic Arts Daily site.

 

It is not that difficult to learn and you will enjoy the process. It involves coating the pot with a thin slip then rubbing it until it shines. It is a low fire process.

Share this post


Link to post
Share on other sites

Wow, I am really impressed with the speed and interest of the replies! Thank you!! Min, you're correct. This is indeed Mathieu Casseau. We saw him at a show here in France over the weekend (I'm originally from Canada :) ) Here's a couple more pics from the weekend.

post-77169-0-64749100-1462729026_thumb.jpg

post-77169-0-94793000-1462729027_thumb.jpg

post-77169-0-64749100-1462729026_thumb.jpg

post-77169-0-94793000-1462729027_thumb.jpg

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.