Morning all,

 

I recently ordered a glaze which was available in matt and glossy.  I unfortunately did not specify the glossy code and the supplier did not check with me regarding the two options. I ordered 5kg and I really don't want to purchase another 5kg, as I had already made it up.  Can anyone suggest what I can add to this to make it glossy.

 

Thanks in advance

 

Andrea

Share this post


Link to post
Share on other sites

If you have a clear glossy, could test  over dipping a thin coat . I'd only do this on the top  third of a pot, or better on a test pot/tile.

Production glaze, have you the recipe?.

Even though this is disappointing maybe order hte glossy and play with the two similar glazes on pots, could be interesting:-00

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.