I was using masking tape to mask an area and put it under a heat lamp to speed my process, but managed to melt a little of the adhesive onto the bisque.  

 

Do I need to fire the plate once with the underglaze to get the adhesive off and then add the clear glaze?  Do I need to treat this adhesive like wax?

 

You can see the adhesive in the picture below.  I attempted scraping it off and was able to get some of it up, but not all.

 

THANK YOU!

post-73693-0-92193100-1456888702_thumb.jpg

post-73693-0-92193100-1456888702_thumb.jpg

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.