cal36 0 Posted December 23, 2015 Report Share Posted December 23, 2015 Hi I am busy working on some ballerina figures and would like to make a flesh-like shiny brown glaze for them-but with some variegated effects in the glaze, and need quite a thick, smooth finish. have tried a few recipes unsuccessfully Can anyone help please? Carol Link to post Share on other sites
bciskepottery 963 Posted December 23, 2015 Report Share Posted December 23, 2015 We need to know your firing range -- 06, 05, 04, 6, 10 -- before you can get an answer. And, firing in oxidation or other atmosphere. Link to post Share on other sites
MatthewV 259 Posted December 24, 2015 Report Share Posted December 24, 2015 Rutile helps with variegation (0-6%) Iron is the most common brown (5-10%) Adding a little manganese might also be desirable (0-2%) And my quick opinion on the ranges I might play with. Link to post Share on other sites
cal36 0 Posted January 5, 2016 Author Report Share Posted January 5, 2016 Thanks I am firing at equivalent cone 6 in an electric kiln, using stoneware paperclay. Link to post Share on other sites
Recommended Posts
Archived
This topic is now archived and is closed to further replies.