cal36 0 Posted December 23, 2015 Report Share Posted December 23, 2015 Hello I have made a beautiful gold flecked glaze but it is too runny! How can i fix it? Carol Link to post Share on other sites
Min 3,429 Posted December 23, 2015 Report Share Posted December 23, 2015 Increase the alumina and/or decrease the flux. Simple fix would be to run a line blend and add more clay, starting with 2% more and going up by 2% until it stops running. Any chance it is runny from overfiring? If you post the recipe it would help with giving more specific suggestions. Link to post Share on other sites
neilestrick 4,592 Posted December 23, 2015 Report Share Posted December 23, 2015 If you find that adding just clay is causing it to get too matte, add equal parts clay and flint, and your silica/alumina ratio won't change much. Link to post Share on other sites
cal36 0 Posted January 5, 2016 Author Report Share Posted January 5, 2016 thank you very much Carol Link to post Share on other sites
Recommended Posts
Archived
This topic is now archived and is closed to further replies.