I don't use a kiln sitter but from what I remember that others have said on here bars sit more evenly in the sitter where its easier to place a cone slightly off center which will affect how it works.

 

Paul

Share this post


Link to post
Share on other sites

In addition to the uniform physical dimensions of the bar vs. the variable thickness of the cone, the bars are designed to run a little hotter than the same number cone, to account for the additional heatwork flowing up and down the side edges of the kiln vs. in the middle of a shelf. The possible downside is that many walk-in supply shops do not carry the bars, only the mini-cones. If yours is one of the few that does carry them, you are in luck; otherwise you will need to order them from one of the usual online suspects.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.