Guest JBaymore

It adds some silica into the melt, and causes localized reduction within the melt. The outgassing can cause a lot of bubbles in the glaze, and it can be used decoratively for "crater glazes".

 

best,

 

.................john

Share this post


Link to post
Share on other sites
Guest HerbNorris

Here is a glaze from the Ceramic Arts Daily e-book "10 tried and true low -fire glaze recipes" It fires at cones 08-04.

 

 

post-5755-13126566438897_thumb.jpg

post-5755-13126566438897_thumb.jpg

Share this post


Link to post
Share on other sites

It adds some silica into the melt, and causes localized reduction within the melt. The outgassing can cause a lot of bubbles in the glaze, and it can be used decoratively for "crater glazes".

 

best,

 

.................john

 

 

 

thank you very much

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.