I am trying out an American recipe for magic water, which includes soda ash, water and soda silicate.

Is soda ash the same thing as bicarb soda i use in the kitchen? perhaps the terminology is different in Australian recipes?

diane solomon westerhuis (the Protean Shed)

Share this post


Link to post
Share on other sites

But,you can make soda ash by calcining the baking soda. In fact just place the baking soda in a frying pan and heat it on high. The extra CO2 will start to "bubble out" of the baking soda. stur until no new gas bubbles form. You now have soda ash, sodium carbonate. Make sure to keep it in a sealed container after heating.

 

Jed

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.