vika 0 Posted July 6, 2011 Report Share Posted July 6, 2011 I am wanting to fire a glazed ball and wonder how to do so without it sticking to the shelf. would anyone have any ideas? many thanks. Link to post Share on other sites
Matt Katz 15 Posted July 6, 2011 Report Share Posted July 6, 2011 wire stilts is your best bet Link to post Share on other sites
Chris Campbell 1,226 Posted July 6, 2011 Report Share Posted July 6, 2011 I agree with Matt ... Those simple stilts with wires will leave only a tiny mark that you can easily sand off. Link to post Share on other sites
acg 0 Posted July 6, 2011 Report Share Posted July 6, 2011 The stilts are made for different temp. firing. Make sure you buy the ones that match your firing. Link to post Share on other sites