I mixed up a small test batch of a the Chinese crackle glaze I found a recipe for in another topic.

As follows:

83 Custer feldspar

8 silica

9 whiting

Add 10 Zircopax

 

However, this glaze won't stay in suspension very long - starting to settle almost before I can get the lid off and start applying.

Anything I can do to help matters?

Thanks!

Share this post


Link to post
Share on other sites

I mixed up a small test batch of a the Chinese crackle glaze I found a recipe for in another topic.

As follows:

83 Custer feldspar

8 silica

9 whiting

Add 10 Zircopax

 

However, this glaze won't stay in suspension very long - starting to settle almost before I can get the lid off and start applying.

Anything I can do to help matters?

Thanks!

 

 

Glazes require 5-10% clay for suspension.

 

That would alter your formula substantially.

try 1-2 % bentonite as an alternative.

Share this post


Link to post
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

Sign in to follow this  

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.