Hello!
I recently purchased some Laguna Speckled Buff (WC-403) and have been throwing some pieces on the wheel. I have been looking for a perfect honey brown/light tan speckled clay and finally came across this one. Anyway, I made and fired some pieces with a Cone 6 cone in the kiln sitter and everything turned out kind of burned (?) looking and darker than I was expecting. I fired some more pieces but this time put a Cone 5 bar in the kiln sitter and got almost the same result My glazes also aren't showing up as well. Does anyone have any ideas of why it is coming out like this or have any advice?
Thanks a bunch!