Jump to content

Search the Community

Showing results for tags 'standard clay'.

  • Search By Tags

    Type tags separated by commas.
  • Search By Author

Content Type


Forums

  • Ceramic Arts Daily Forums
    • Forum FAQ & Terms of Use
    • Studio Operations and Making Work
    • Clay and Glaze Chemistry
    • Mold Making and Slip Casting
    • Equipment Use and Repair
    • Business, Marketing, and Accounting
    • Educational Approaches and Resources
    • Aesthetic Approaches and Philosophy
    • Int'l Ceramic Artists Network (ICAN) Operations and Benefits
    • Ceramic Events of Interest
    • Community Marketplace – Buy/Sell/Trade/Free
    • Job and Career Opportunities

Find results in...

Find results that contain...


Date Created

  • Start

    End


Last Updated

  • Start

    End


Filter by number of...

Joined

  • Start

    End


Group


AIM


MSN


Website URL


ICQ


Yahoo


Jabber


Skype


Location


Interests

Found 2 results

  1. I have been having a strange issue with my Cone 6 Black Stoneware Clay from Standard (266). It gets these big cracking bubbles upon glaze firing. I bought this clay to marble with Porcelain (Standard 365) because it had a similar shrink rate. The marbled pieces came out SUPER bubbly, really horrible. I thought it was just poor clay preparation on my part because of the mixing of the two. However it has been happening with pots I make solely out of the Black Stoneware. I prepare this clay the same way I do all my other clay bodies and never really have this issue otherwise. Has anyone else had this problem with this clay? Any advice?
  2. Hello! Does anybody have experience firing Standard Clay 112 or 182 to cone 06/6? These are the clays that I work with and typically my studio fires to cone 05/5. However, I have recently started working out of home and found a studio nearby that will fire my work, but to cone 06/6. I want to be sure that I like the result before committing to the change.
×
×