Hi there. I recently glazed some items on white stoneware clay.
The clay (White Stoneware PF560) was glazed fired after being bisqued at :
room --> 600 degrees C at 100 deg/c per hour
600 -> 1230 at 150 deg/c per hour
20 min soak
It came out really patchy and there are some air bubbles. If anyone could recommend good firing ramp for this glaze in degrees celcis with timing that would be great - thanks so much
Terracolor orange Ember - https://www.scarva.com/en/gb/Terracolor-FS6031-Orange-Ember/m-1772.aspx was the glaze that didnt look very good!
Clay was : https://www.bathpotters.co.uk/white-stoneware-pf560