Jump to content

Search the Community

Showing results for tags 'mug'.

  • Search By Tags

    Type tags separated by commas.
  • Search By Author

Content Type


Forums

  • Ceramic Arts Daily Forums
    • Forum FAQ & Terms of Use
    • Studio Operations and Making Work
    • Clay and Glaze Chemistry
    • Mold Making and Slip Casting
    • Equipment Use and Repair
    • Business, Marketing, and Accounting
    • Educational Approaches and Resources
    • Aesthetic Approaches and Philosophy
    • Int'l Ceramic Artists Network (ICAN) Operations and Benefits
    • Ceramic Events of Interest
    • Community Marketplace ā€“ Buy/Sell/Trade/Free
    • Job and Career Opportunities

Find results in...

Find results that contain...


Date Created

  • Start

    End


Last Updated

  • Start

    End


Filter by number of...

Joined

  • Start

    End


Group


AIM


MSN


Website URL


ICQ


Yahoo


Jabber


Skype


Location


Interests

  1. Is it possible to attach a small dry handle to a wet casted cup? Iā€™d think yes, but wonder if anyone does their production this way. Thanks for sharing your wisdom
  2. From the album: rdimes projects

    blue mug and cup set clay: light stoneware? glaze: ? techniques: wheel thrown, cups made off the hump start date: ? completion date: 2019 location: mug and two cups gifted to Gabriela, remaining two cups in my appt
  3. rdimes

    teadust mug

    From the album: rdimes projects

    tea dust mug clay: light stoneware glaze: tea dust 2/3 dip over tyler exterior, blue celadon interior techniques: wheel thrown start date: summer 2021 completion date: August 18, 2021 location: gifted to Kate M in Feb 2022
  4. How many roughly 1 lb mugs of the same size and shape can you throw in an hour? I'm looking to hire an assistant to do piece work for me and I need to get a realistic baseline and expectation of what I should expect and how much I can pay per piece.
  5. From the album: Mug inspired in vintage enamelware

    multiple uses for one mug
  6. Guest

    Burnish Gold Luster Mug

    From the album: John Baymore's Clay Work

    This cup is in the invitational exhibition "I'll Drink To That" at the Eclipse Mill Gallery in North Adams, MA until August 27th, 2017. Handbuilt, woodfired, American Shino, overglaze enamel, gold luster.

    © 2017 - John Baymore - all rights reserved

  7. From the album: Favorites

    I love all the varied shapes a good mug comes in. The shape is my current favorite. It works well to separate the textured areas from the geometric sgraffito in the bottom. It has a pulled handle and commercial glazes and was fired to cone 6 electric.
  8. From the album: Custom Mugs and Commission Concepts

    Handbuilt stoneware mugs, approximately 12oz capacity, fired cone10. Surface treatment includes 3-d dwelling, carved-out hillside community, and underglaze image transfers. The transfers are new to me...using a CriCut Explore to create silkscreen masks through which thickened underglaze is printed onto rice paper. Once dried, the surface of the mug is coated in underglaze, the transfer is sprayed until saturated, and then pressed/burnished (with pint side to the mug) onto the bisque fired surface. I'm not yet comfortable enough with this technique to try it on greenware but it should work equally well. Certainly there is a story to these mugs...the short version centers around work in some of the poorest slums in Central/South America in contrast with visits to numerous iconic cites in Europe.

    © Copyright 2016 - Paul M. Chenoweth, Nashville, Tennessee USA. All rights reserved.

  9. From the album: Custom Mugs and Commission Concepts

    This is a 14oz-16oz wheel-thrown, stoneware mug with slab-built (black only) keys attached to a carved/altered keyboard design. The handle idea is NOT original but borrowed/copied/altered from another artist's project. When I find the name, I will certainly give proper attribution. Interior is glazed with Woo's Blue. Exterior details are black and white, brushed-on, Amaco Velvet underglazes with a top coating of clear. This is a concept mug for a commissioned gift project that is currently underway. The basic form and structure may remain the same but the color scheme for the actual project will be altered considerably.

    © Copyright 2017 - Paul M. Chenoweth, Nashville, TN USA - All rights reserved.

  10. From the album: Custom Mugs and Commission Concepts

    Handbuilt stoneware mug, approximately 12oz capacity, fired cone10. Surface treatment includes 3-d dwelling, carved-out hillside community, and underglaze image transfers. The transfers are new to me...using a CriCut Explore to create silkscreen masks through which thickened underglaze is printed onto rice paper. Once dried, the surface of the mug is coated in underglaze, the transfer is sprayed until saturated, and then pressed/burnished (with pint side to the mug) onto the bisque fired surface. I'm not yet comfortable enough with this technique to try it on greenware but it should work equally well. Certainly there is a story to these mugs...the short version centers around work in some of the poorest slums in Central/South America in contrast with visits to numerous iconic cites in Europe.

    © Copyright 2016 - Paul M. Chenoweth, Nashville, Tennessee USA. All rights reserved.

  11. From the album: Custom Mugs and Commission Concepts

    Handbuilt stoneware mugs, approximately 12oz capacity, fired cone10. Surface treatment includes 3-d dwelling, carved-out hillside community, and underglaze image transfers. The transfers are new to me...using a CriCut Explore to create silkscreen masks through which thickened underglaze is printed onto rice paper. Once dried, the surface of the mug is coated in underglaze, the transfer is sprayed until saturated, and then pressed/burnished (with pint side to the mug) onto the bisque fired surface. I'm not yet comfortable enough with this technique to try it on greenware but it should work equally well. Certainly there is a story to these mugs...the short version centers around work in some of the poorest slums in Central/South America in contrast with visits to numerous iconic cites in Europe.

    © Copyright 2016 - Paul M. Chenoweth, Nashville, Tennessee USA. All rights reserved.

  12. From the album: Ceramics Fall 2016

    I made 4 similar mugs from the recycled clay and iron filings in a glaze called moonlight. I have learned that a little goes a long way for the iron filings, and next time I think I will use less. Most of the filings came through on the inside of the cup, rusting slightly but covered thinly by glaze. Does any one else have experience with using too much iron filings? Do you feel it causes any safety hazards to the average human?
  13. From the album: Custom Mugs and Commission Concepts

    This is a 12oz-14oz. stoneware mug with a piano/keyboard theme. The rim is wheel thrown and re-assembled into a hand-built, slab-constructed base that has been stamped and stretched/altered. Handle is pulled and attached after the rim is in-place and black keys have been cut from a slab and attached/scored & slipped. Interior and rim is glazed with Woo's Blue. Exterior parts are brushed-on Amaco Velvet underglaze sprayed with a couple of light coats of clear. Mug is fired to Cone 10 reduction. This is a concept mug, developed for Nashville's music scene and various associated festivals. The design includes the possibility of a custom name imprint along the top edge of the slab construction. Estimated retail would be around $60.

    © Copyright 2017 - Paul M. Chenoweth, Nashville, TN USA - All rights reserved.

  14. From the album: Fun Fun Fun

    © Pottery by Penny

  15. From the album: Favorites

    This was a new take on a design I've been doing awhile. It may have spurred a new variation on several of my usual pots. I'm excited to see what comes of it. The pattern at the bottom was created with paper resist and sgraffito. After bisque fired, black underglaze was applied and wiped back, then colorful accents added to the wings. It's finished with commercial ial glazes and fired to cone 6 in an electric kiln.
  16. From the album: Favorites

    Wheel thrown and hand carved. The bottom features a leaf design created by using paper leaves as a resist to the underglaze. Sgraffito designs were added along with a pulled handle and spiral embellishments. Fired to cone 6 in an electric kiln.
  17. From the album: Favorites

    This one is fresh from my latest firing. I'm in love with this one. It's wheel thrown with a pulled handle, underglaze decoration, and hand carved texture. It's glazed in 3 different commercial glazes and fired in my electric kiln.
  18. From the album: Rogryphon's stuff

    Continuing on the bubble bandwagon a mug.
  19. From the album: "Lifestyle" Images for Online Selling

    Added the burlap placemat, changed the spoon, repositioned the tea bag tag. Kept the spoon and tea bag tag for scale.

    © Terry Buffington

  20. From the album: Custom Mugs and Commission Concepts

    A small set of hand-built mugs (slab construction) with wheel-thrown rims for family friends...both of whom are musically gifted. The orange has a look of atmospheric firing, but it is actually Amaco Velvet orange underglaze. The sheen over the underglaze is from a light coating of clear. The interior and rim were dipped in Woo's Blue. The details on the piano keys are brushed on. All of the rest of the glazing was sprayed. These are 12oz (.35ml) and stand approximately 5in. (12.7cm) tall. These were fired to Cone 10 in reduction.

    © Copyright 2016 - Paul M. Chenoweth - Nashville, TN USA All rights reserved.

×
×