It looks like some of my shelves are hitting temp but kiln sitter hasn’t been triggering auto shut off (pyrometric bar melting). Please advise TIA!
-
So any tips for preventing warping on a cone 4 ( yes I mean 4 not 04 :D ) vitreous slip cast clay? It's a tall tiki form that is a little top heavy so they wants to sag/warp. I'm applying amaco velvet underglaze to the exterior that develops a slight sheen so I don't want to lay them on their side... Also has anyone tried firing amaco celedons at cone 4? I've been experimenting with some recipes but they are coming out more opaque and milky. Kinda in a crunch!
-
From the album: MOAR STUFFS
This was a piece I did in college--I sure miss midrange firing. Sadly, the postal worker who delivered this big bowl to the lady who ordered it from me just slammed the box it was in on her cement porch, and my beautiful work broke in three pieces. :'( GAH... Fired to ^6 in a Skutt electric. White stoneware.© The Earthen Cavy/Sarah Alderete