Hello and thank you in advance for any of you that might be able to give me an advice. I am looking for a solution to transport overglazed items ( luster, to be precise ). I have already found a method for raw ( sawdust ) and another for the glazed items ( cornstarch spray ). I am wondering if the cornstarch spray method would work also with the lusters or is there any reaction between the substances that would not recomend this method. Or perhaps you have used other methods and something worked. I very much thank you!