From the album: Hyn Patty LLC
3.5 inch tall earthenware ceramic sculpted by Maureen Love and produced by Hagen Renaker. Custom glazed to liver chestnut sabino pinto by Hyn Patty, 2021. Underglaze, clear satin, glossed eyes and hooves, china paints. Claybody customized resculpting and repaired broken legs done in the kiln to the bisque before glazing. Shown here sticky mounted to base.