From the album: Sketches by Paul
Realizing that the greenware portions of the container will all of the assembled parts will weight 12-14 pounds, I changed the plans for the base to be more than just stocky feet. This will dry slowly over night since the wheel thrown pieces and the hand built feet are at different degrees of dryness. All together, the bas will have to be quite dry before assembling the top to the base.